18 – Mastertig AC/DC 2000, 2500, 2500W, 3500W/0510 © COPYRIGHT KEMPPI OYBALANCE2.4 3.24.0ACACFREQUENCY50 - 200 HzMINILOGOFF-80%+20%21a. When welding with a sharpened electrode, turn the controlknob to the left edge of the range of the electrode that youhave selected. (Narrow arc, deep penetration, range: smallseams)1b. When welding with a rounded electrode, turn the control knobto the right edge of the range of the electrode that you haveselected.2. If you want more heat to the electrode, turn the knob to theright, or if you want less heat, turn it to the left.3.4.9. Frequency adjustment of TIG AC welding(only with minilog and pulse panel)The frequency of AC welding can be adjusted by means of the MINILOG and PULSE PANEL.Raising the frequency will make the arc slightly more stable and narrow, but it will increase thenoise caused by arc.1. Press the FREQUENCY key in the AC square.2. Adjust the frequency with the current knob. The adjustment range of thefrequency is 50 ... 200 Hz. When leaving the factory, the frequency of themachine is 60 Hz.3.4.10. Minilog operation (only with minilog and pulse panel)With the Minilog operation you can select two currency levels, the weldingcurrent and the base current, and you can move from one to the other by quicklypressing the torch. The Minilog operation can be used only with a 4-function torchswitch operation.The selection and adjustment of the Minilog operation is done by means of thepotentiometer. When the potentiometer is in the OFF position, the operation isnot in use. The welding current is selected from the current knob like usually. TheMinilog knob is used to select a basic current, the minimum of which is 80 %You can move from the welding current to the basic current by quickly pressing the torch.By quickly pressing it again, you move back to the welding current. The signal lights on thepanel show you the current level you are on.You can stop the welding by a longer pressing of the torch switch (> 0.7 s).The Minilog operation can be used to adjust the heat, if the work piece is overheated or if youneed more heat for a moment.With the Minilog operation you can go to a lower current level for example when you changethe position or the grip of the filler material wire without having to stop the welding to do that.A lower current can also be used as the crater filling current if you do not want to use the down-slope time for that.below the welding current and the maximum is 20 % above thecurrent level. During the adjustment, you can see the set value ofcurrent in amperes in the current display.